The Nb-10Si (mole fraction, %) alloy was fabricated using the vacuum arc-melting method and heat-treated at 1850 ℃ and 1550 ℃ for 2~100h in Ar at mosphere. The
Extraction of copper from bacterial leach solution using Lix984 had been performed.It was found that the main factors influencing extraction yield of copper are