Mg-3.99Y-3.81Nd-0.53Zr(WE43)casting alloy was subjected to single-pass friction stir processing(FSP)at a constant processing speed of 60 mm?min-1 and various ro
The extruded Mg-7Y-1Nd-0.5Zr(wt%)alloy were performed to the same strain hot rolling with different temperatures.The microstructure and texture evolution of the